Friday, May 6, 2016

Week 4: 4/22 - 4/28

This week, we wrote a detailed step-by-step procedure (including materials) for the production of chitosan layered alginate beads; more details can be found under the materials & methods tab. Essentially, we will be mixing 3% w/v sodium alginate into 3% w/v calcium chloride dropwise with a size 22 syringe to form small beads. Then, we will stir the beads in antacid solution to encapsulate the therapeutics. Finally, we will dip each bead into chitosan solution for < 1 second and wash them with distilled water to form the polyelectrolyte complex film.

Related Posts:

  • Week 8: 5/20 - 5/26This week, we continued testing from the previous week. A control group of ordinary loaded calcium alginate beads were placed in a neutral and acidic environment as well; it serves as a baseline for our chitosan-coated b… Read More
  • Week 5: 4/29 - 5/5This week, we ordered our materials for the production of chitosan layered alginate beads. Specifically, we ordered 50 mL of chitosan solution (which we will dilute to 3% w/v), a syringe with size-22 needle, several 50 mL and… Read More
  • Week 6: 5/6 - 5/12This is the first week of experiments. We are doing a preliminary experiment to test our method today during lab. Several chitosan-coated alginate beads were successfully created. … Read More
  • Week 4: 4/22 - 4/28This week, we wrote a detailed step-by-step procedure (including materials) for the production of chitosan layered alginate beads; more details can be found under the materials & methods tab. Essentially, we will be … Read More
  • Week 7: 5/13 - 5/19This is the second week of experiments and first week of testing. The same procedure as last week was followed to create the chitosan alginate beads. Half of the chitosan alginate beads was placed in 20 mL of water, while the… Read More